Nov 20, 2026 Leave a message

20 Tons 1050 O Aluminum Strip Coil 0.5mm X 365mm Burr Free For Vietnam Transformer Winding

A transformer manufacturer based in Ho Chi Minh City, Vietnam, placed a trial order of 20 tons of aluminum strip coil for dry type transformer winding. The material specification was tight: 1050 alloy in O temper, 0.5mm thickness, 365mm width, with perfectly smooth slit edges, no burr and no edge waviness, and a flawless mill finish surface. This case explains how the order was produced, inspected and shipped in 12 working days.

 

 

Customer Background

 

The buyer produces distribution transformers and dry type transformers for the Vietnamese power grid and industrial projects. Aluminum foil and strip windings are used in low voltage windings where conductivity, winding tightness and insulation integrity are critical. Their previous supplier delivered coils with slight edge burr and wave, which caused foil tearing during high speed winding and forced the client to stop the line and re-slit the material locally.

 

 

Requirements

 

  • Alloy and temper: 1050 in O temper for maximum softness and elongation during winding
  • Dimension: 0.5mm thickness x 365mm width, coil ID 76mm, coil weight 2-3 tons
  • Edge quality: smooth slit edge, no burr, no wave, no camber
  • Surface: flawless mill finish, no scratch, no oil stain, no inclusion
  • Quantity: 20 tons for the first shipment
  • Delivery: within 15 days to Cat Lai port, Ho Chi Minh City

 

 

Product Specification

 

Item Specification Test Method
Alloy 1050 Spectrometer analysis
Temper O (annealed) GB/T 3880.1-2006
Thickness 0.5mm +/-0.01mm Micrometer, 5 points per coil
Width 365mm +/-0.3mm Steel tape, 3 points per coil
Tensile Strength 60-95 MPa ASTM E8 / GB/T 228
Elongation 25% minimum ASTM E8 / GB/T 228
Coil ID 76mm Gauge
Coil Weight 2-3 tons per coil Platform scale
Surface Mill finish, no scratch, no stain Visual inspection under 300 lux

 

 

Production and Quality Control

 

The coil was rolled from 1050 aluminum ingot on our cold rolling line, annealed to O temper in a batch annealing furnace to reach the required softness, then slit on a precision slitting line with tension control to avoid edge wave. The complete process took 9 working days from order confirmation.

 

  • Slitting control: tungsten carbide slitting knives, knife clearance set to 3% of thickness, tension and speed optimized for 0.5mm soft strip to eliminate burr and wave
  • Edge inspection: every coil checked under magnification, burr height controlled below 0.02mm, camber below 1mm per meter
  • Surface inspection: 100% visual check under 300 lux lighting, both surfaces, no scratch, no oil stain, no rolled in inclusion
  • Thickness and width: 5 thickness points and 3 width points recorded per coil, all results attached to the mill test certificate
  • Packaging: eye to sky on seaworthy wooden pallet, paper interleave and PVC film, edge protector, steel strapping, moisture proof wrapping

 

2026112017410354752

 

Results

 

Metric Before (previous supplier) After (Yongsheng)
Edge burr Visible burr, occasional foil tearing Burr below 0.02mm, no tearing
Edge wave Wave causing winding misalignment No wave, straight edge
Winding line stoppage 2-3 times per shift Zero stoppage after switch
Material rejection rate About 3% Below 0.3%
Lead time 25-30 days 12 working days

 

The client confirmed the coils passed incoming inspection without any rework. The winding line ran continuously without a single stoppage caused by material defects, and the rejection rate dropped from about 3% to below 0.3%. Based on this first 20 ton shipment, the buyer scheduled a follow up order of 40 tons for the next quarter and added 1060 O and 1070 O strip coils in 0.3mm and 0.8mm to the same supply agreement.

 

 

Why This Matters for Transformer Winding

 

In transformer winding, aluminum strip is wound at high speed under constant tension. Any burr on the slit edge acts as a stress riser and can cut through the interleaved insulation paper, while edge wave causes the strip to ride up and misalign the winding. A flawless surface also matters, because scratches and inclusions can create partial discharge points inside the winding. Controlling burr below 0.02mm, camber below 1mm per meter and oil residue to zero is therefore not a cosmetic requirement, but the core of winding reliability.

 

 

Product and Service Highlights

 

  • 1050, 1060, 1070 and 1100 aluminum strip coil in O, H14, H18 and H24 temper
  • Thickness from 0.1mm to 6.0mm, width from 10mm to 1600mm with custom slitting
  • Burr free precision slitting with tension control, suitable for foil winding machines
  • Free sample coil for winding trial before bulk order
  • Mill test certificate, SGS or BV third party inspection on request
  • ISO 9001:2015 certified production, 450,000 tons annual capacity, export to more than 60 countries

 

If you are sourcing aluminum strip coil for transformer winding, reactor winding or foil wound inductors, send your thickness, width, temper and edge requirement, and we will confirm the specification and quotation within 12 working hours.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry